MORTAR
Single component rendering mortar with a ratio of graded inert sand with cement and polymers for applications in civil construction works.
Less water consumption
Increase in durability
Reduce Rebound losses
| Properties | Results |
|---|---|
| Pot life at 300C min | 90 - 120 |
| Compressive Strength at 28 days. Mpa | 6 - 8 |
| Tensile Strength at 28 days. Mpa | Min.1.0 |
| Flexural Strength at 28 days. Mpa | Min.1.5 |
| Water Absorption% | Max 5 |